RESIN BONDING CEMENT WITH CHEMICAL SELF-POLYMERIZATION FUNCTION INDICATIONS: Bonding of indirect restorations (inlays, onlays, crowns, bridges, and posts). ¨ Metal-ceramic crowns & bridges. ¨ All-ceramic crowns & bridges made of lithium disilicate. ¨ Maryland type bridge veneers. ¨ Bonding of implant-supported restorations (abutments). PRODUCT BENEFITS: ¨ Comfortable handling with the auto-mixing system. ¨ Satisfactory self-curing time. Elastic phase 2 - 2.5 minutes. Total setting time 4 minutes. ¨ Saving working time. No etchants, activators, or adhesives needed. ¨ High bond strength in cohesive forces under compression (195-200MPa) and tensile strength in both metal and ceramic. ¨ Low solubility in oral fluid acids. ¨ Restorations do not discolor. TECHNICAL INFORMATION: 1) Self-curing time 2 - 2.5 minutes. 2) Setting time 3 - 4 minutes 3) Compressive strength 195-200MPa 4) Viscosity thickness 35mm